PENGARUH PENAMBAHAN CANGKANG KEONG (FLY ASH) DENGAN PERSENTASE 1%, 2% DAN 3% DAN SIKACIM CONCRETE ADDITIVE SEBESAR 0,7% TERHADAP KUAT TEKAN BETON THE EFFECT OF ADDITIONING CONCH SHELL (FLY ASH) WITH PERCENTAGE 1%, 2% AND 3% AND A MASSIVE CONCRETE ADDITIVE SYSTEM 0.7% AGAINST THE STRENGTH OF CONCRETE PRESS

Alfiona, Vera and Budianto Kromodiryo, Johan (2021) PENGARUH PENAMBAHAN CANGKANG KEONG (FLY ASH) DENGAN PERSENTASE 1%, 2% DAN 3% DAN SIKACIM CONCRETE ADDITIVE SEBESAR 0,7% TERHADAP KUAT TEKAN BETON THE EFFECT OF ADDITIONING CONCH SHELL (FLY ASH) WITH PERCENTAGE 1%, 2% AND 3% AND A MASSIVE CONCRETE ADDITIVE SYSTEM 0.7% AGAINST THE STRENGTH OF CONCRETE PRESS. Tugas Akhir thesis, University of Technology Yogyakarta.

[img]
Preview
Text
ABSTRAK_5160811100_Vera Alfiona .pdf

Download (212kB) | Preview

Abstract

ABSTRAK Beton merupakan salah satu bahan bangunan yang paling banyak digunakan di Indonesia. Inovasi diperlukan untuk meningkatkan mutu beton dalam hal kuat tekan beton. Inovasi yang dilakukan dalam penelitian ini adalah penambahan limbah cangkang keong sebagai fly ash dengan persentase 1%, 2% dan 3% dan bahan tambah sikacim concrete additive sebesar 0,7% pada beton. Tujuan dari penelitian ini adalah untuk mengetahui pengaruh penambahan fly ash cangkang keong dan penggunaan sikacim concrete additive terhadap dan nilai slump, beban maksimal, dan kuat tekan beton. Metode pengujian dilakukan di Laboratorium PT. Aneka Dharma Persada. Pembuatan benda uji yang digunakan yaitu silinder yang terdiri dari 3 beton normal dan 9 beton fly ash cangkang keong dengan tambahan sikacim concrete additive, dengan umur 28 hari dengan mutu rencana 20 Mpa. Persentase penambahan fly ash cangkang keong yaitu sebesar 1%, 2%, dan 3%, sedangkan penambahan sikacim concrete additive yaitu sebesar 0,7%. Hasil pengujian nilai slump pada beton normal adalah 10 cm, sedangkan beton dengan penambahan fly ash cangkang keong 1%, 2% dan 3% dengan sikacim concrete additive 0,7% yaitu sebesar 10 cm, 11 cm dan 11 cm. Nilai rata-rata beban maksimal pada beton normal yaitu sebesar 423 kN, sedangkan beton dengan penambahan fly ash cangkang keong 1%, 2% dan 3% dengan sikacim concrete additive 0,7% yaitu sebesar 547 kN, 464 kN, dan 438 kN. Nilai rata-rata kuat tekan beton normal adalah 23,933 MPa, sedangkan beton dengan penambahan fly ash cangkang keong 1%, 2% dan 3% dengan sikacim concrete additive 0,7% adalah sebesar 30,983 MPa, 26,270 MPa dan 24,800MPa. Kata Kunci: Sikacim Concrete Additive, Cangkang Keong ABSTRACT Concrete is one of the most widely used building materials in Indonesia. Innovation is needed to improve the quality of concrete in terms of the compressive strength of concrete. The innovations carried out in this study were the addition of conch shells as fly ash with the percentage of 1%, 2% and 3% and the added material of sikacim concrete additive of 0.7% to the concrete. The purpose of this study was to determine the effect of adding conches shell fly ash and the use of sikacim concrete additive to the slump value, maximum load, and compressive strength of the concrete. The test method is carried out at the laboratory of PT. Various Dharma Persada. The test object used is a cylinder consisting of 3 normal concrete and 9 conch shell fly ash concrete with additional additive sikacim concrete, with an age of 28 days with a plan quality of 20 MPa. The percentage of addition of conch shell fly ash was 1%, 2%, and 3%, while the addition of sikacim concrete additive was 0.7%. The test results of the slump value in normal concrete are 10 cm, while the concrete with the addition of 1%, 2% and 3% conch shell fly ash with 0.7% sikacim concrete additive is 10 cm, 11 cm and 11 cm. The maximum average load value of normal concrete is 423 kN, while the addition of 1%, 2% and 3% of the conch shell fly ash with 0.7% sikacim concrete additive is 547 kN, 464 kN, and 438 kN. The average value of the compressive strength of normal concrete is 23,933 MPa, while the addition of 1%, 2% and 3% addition of fly ash conch shells with 0.7% sikacim concrete additive is 30,983 MPa, 26,270 MPa and 24,800MPa. Keywords: Sikacim Concrete Additive, Conch Shell DAFTAR PUSTAKA Aida, Tria Nur. (2020). Pengaruh Substitusi Limbah Cangkang Telur (Fly Ash) Dengan Persentase 4%, 5%, Dan 6% Dan Kain Perca Sebesar 2% Sebagai Bahan Tambah Pada Beton Terhadap Kuat Tekan. Universitas Teknologi Yogyakarta. ASTM. C 33-82, Standard Specification for Concrete Aggregate, ASTM, Book of Standards, USA. Badan Standarisasi Nasional Indonesia. (1982). Persyaratan Umum Bahan Bangunan di Indonesia (PUBI-1982) Pasal 11 tentang Pasir. Jakarta:BSN. Badan Standarisasi Nasional. (2004). SNI 15-2049-2004. Semen Portland. Bandung: BSN. Delvita Haryona, Djusmaini Djamas dan Ramli. (2015). Pengaruh Variasi Temperatur Kalsinasi Terhadap Karakteristik Kalsium Karbonat (CaCO3) Dalam Cangkang Keong Sawah (Pilla ampullaceal) yang Terdapat di Kabupaten Pasaman. Vol 6, 17-24. Hartantyo, Sugeng Dwi dan Muhammad Hakim Susianto. (2019). Pengaruh Penambahan Tumbukan Cangkang Keong Mas Terhadap Kuat Tekan Beton Non Struktual K-175. Vol. 3, p ISSN 2579-4620, e issn 2581-0855. Jamal Mardewi, Masayu Widiastuti dan Anggi Tossib Anugrah. (2017). Pengaruh Penggunaan Sikacim Concrete Additive Terhadap Kuat Tekan Beton Dengan Menggunakan Agregat Kasar Bengalon Dan Agregat Halus Pasir Mahakam. Lincolen, Kevin. (2017). Pengaruh Abu Terbang Sebagai Bahan Pengganti Semen Pada Beton Beragregat Halus Bottom Ash. Bandar Lampung. Universitas Lampung. Mulyati dan Aidi Adman. (2019). Pengaruh Penambahan Cangkang Kemiri dan Sikacim Concrete Additive Terhadap Kuat Tekan Beton Normal. Vol. 6 No. 2, P-ISSN 2354-8452, E-ISSN 2614-414X. Novrianti, Rida Respati dan Anwar Muda. (2014). Pengaruh Aditif Sikacim Terhadap Campuran Beton K 350 Ditinjau Dari Kuat Tekan Beton. Nurrizki, Chaulia (2016). Perbandingan Penggunaan Dua Merk Semen PCC Yang Berbeda Terhadap Kuat Tekan. Purwokerto. Universitas Muhammadiyah Purwokerto. SNI 1974:2011. (2011). Cara Uji Kuat Tekan Beton Dengan Benda Uji Silinder Beton. Bandung. Badan Standarisasi Nasional. Supriani, Fepy (2013). Pengaruh umur beton terhadap kuat tekan beton akibat penambahan abu cangkang lokan. Universitas Bengkulu. Tjokrodimulyo, K. (1996). Syarat Gradasi Butiran. Yogyakarta. Biro Penerbit Keluarga Mahasiswa Teknik Sipil Universitas Gajah Mada. Tjokrodimulyo, Kardiyono. (1996). Teknologi Beton. Yogyakarta. Biro Penerbit Keluarga Mahasiswa Teknik Sipil Universitas Gajah Mada.

Item Type: Thesis (Skripsi, Tugas Akhir or Kerja Praktek) (Tugas Akhir)
Subjects: T Technology > TA Engineering (General). Civil engineering (General)
Divisions: Fakultas Sains dan Teknologi > S1 Teknik Sipil
Depositing User: Kaprodi S1 Teknik Sipil UTY
Date Deposited: 30 Dec 2021 08:40
Last Modified: 30 Dec 2021 08:43
URI: http://eprints.uty.ac.id/id/eprint/7408

Actions (login required)

View Item View Item